PLC Splitter Workshop
All cutting procedures adopt automatic cutting, with less error and higher efficiency. After the cutting step, we will strip the fiber and move to next process.
Grinding takes about 15 minutes, then polishing, about 12-15 minutes. After polishing, use a 200-fold magnification detector to check whether the end face is smooth, if not, need to grinding back.
Coupling is the core and key step of PLC production, which needs to be completed in high-level dust-free workshop, and the technical requirements for operators are particularly high.
During whole production process, there are three stages of UV curing. The first one takes 120 seconds to dry the epoxy glue with ultraviolet light. Second, 30 minutes.Third, 30 minutes.After repeated uv curing, ensure that the glue is completely dry.
During whole production process, there are two stages of high temperature baking. Each high temperature bake at 85°C for 8 hours. Ensure that the fiber optic array can maintain the normal operation of the product in high temperature environment.
As the high-low temperature cycle, we put the optical fiber into the environment of -40°C~85°C for the experiment, and it takes 4 hours from the lowest temperature to the highest temperature. Our whole test lasts for 12 hours in total. During the production process, we conduct two cycles of high and low temperature test.
Testing Equipment
Core Calibrator
3D Test
End Face Checking
IL&RL Test
Connect Your Free Samples Soon!